PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
15 sec; ASTM D2240
Tensile Strength, Yield 43.6 MPa
6320 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.28 GPa
476 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 3.35 GPa
486 ksi
ASTM D790
Izod Impact, Notched 4.80 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
8.99 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy 75.6 J/cm

@Temperature 23.0 °C
0.142 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
75.6 J/cm

@Temperature 23.0 °C
0.142 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C

@Thickness 3.18 mm
165 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
Descriptive Properties Value Comments
Ease of Sizing Good
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Profile Extrusion
PVC Cell Classification 1-42234-33-0101
ASTM D4216
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Outdoor Applications