PolyOne Geon™ Vinyl Wire & Cable 8800FR Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable 8800FR Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
15 sec; ASTM D2240
53
53
ASTM D2240
Tensile Strength, Yield 24.1 MPa
3500 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Tensile Modulus 0.0124 GPa
1.80 ksi
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL Temperature Rating
Brittleness Temperature -5.00 °C
23.0 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+12 ohm-cm
1.80e+12 ohm-cm
ASTM D257
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL QMTT2
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Communication Wire Insulation
Communication Wire Jacketing
Wire & Cable Applications
Wire Types THHN
THW
THWN
TW