Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable JG513G2 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable JG513G2 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Deformation 20 %

@Temperature 55.0 °C,
Time 3600 sec
20 %

@Temperature 131 °F,
Time 1.00 hour
200 g; UL 1581
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
15 sec; ASTM D2240
Tensile Strength, Yield 13.8 MPa
2000 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D746
Oxygen Index 25 %

@Thickness 1.91 mm
25 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 160 - 170 °C
320 - 338 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings CSA C-22.2, No. 131
CSA LAG (Low Acid Gas)
Change in Flexural Strength -12%
ASTM D543; 70°C, 1.91 mm; in ASTM Oil #2, 96 hr
Change in Ultimate Elongation -25%
ASTM D543; 70°C, 96 hr, in ASTM #2 Oil; 0.075 in
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
HCL Evolution 13%
CSA C22.2 No. 0.3
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 80%
121°C, 1.91 mm; 336 hr, UL Standard
Retention of Tensile Strength 100%
121°C, 1.91 mm; 336 hr, UL Standard
Uses Wire & Cable Applications
Users viewing this material also viewed the following: