PolyOne LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name LubriOne™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 152 MPa
22000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 228 MPa
33100 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Coefficient of Friction, Dynamic 0.59
0.59
vs. Metal - Dynamic; ASTM D1894
Coefficient of Friction, Static 0.46
0.46
vs. Steel - Static; ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.0 µm/m-°C
18.9 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 254 °C

@Thickness 3.18 mm
489 °F

@Thickness 0.125 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
Descriptive Properties Value Comments
Appearance Black
Features Good Wear Resistance
Lubricated
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Regional Availability North America
RoHS Compliance RoHS Compliant