PolyOne Nymax™ 1308 A HS Natural Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name Nymax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ 1308 A HS Natural Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 1.2 %

@Thickness 3.18 mm
1.2 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
50 mm/min; ISO 527
61.4 MPa
8910 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 65 %
65 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
2.04 GPa
296 ksi
ISO 178
Izod Impact, Notched 1.80 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.37 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C

@Thickness 3.18 mm
149 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Appearance Natural Color
Features General Purpose
Heat Stabilized
Impact Modified
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications