PolyOne Nymax™ GF 1800 43 Natural Nylon 612 with 43% Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ GF 1800 43 Natural Nylon 612 with 43% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molded Test Bars: Dry as Molded
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Filler Content 43 %
43 %
Water Absorption 0.20 %

@Thickness 3.18 mm,
Time 86400 sec
0.20 %

@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 171 MPa
24800 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 3.5 %
3.5 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 210 °C

@Thickness 3.18 mm
410 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C

@Thickness 3.18 mm
392 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Appearance Natural Color
Forms Pellets
Generic Name Polyamide 612 (Nylon 6/12)
Regional Availability North America
South America