Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.28 J/cm @Temperature 23.0 °C |
2.40 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac® 2013A Acetal Homopolymer, UV Stabilized
(discontinued **) Similar to 3013A, but higher in molecular weight.Applications: Pipe fittings, rollers, exterior automotive parts.This product is not a part of the standard product line dated 2003. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | Approximation; ISO 180/1U |
Albis Plastics Tedur® L 9521-1 PPS, 60% Glass Fiber/Mineral
(discontinued **) Extremely Rigid. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Sockets, Plugs and HandlesProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperatur.. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.40 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Nymax™ GF 1880 33 HS NATURAL Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedMolded Test Bars: (Dry as molded:Information provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.40 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Nymax™ GF1800-40 HS Black 13 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedNylon 6/12 CompoundBlackDry as molded:PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC (Asia Pacific) LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific) LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 NAT001 Y 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N330GL (DAM) Nylon 6 (Utility Grade), 30% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature 22.8 °C |
2.40 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Aclo Accucomp ABS ABS881L Clear Grade |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P1440 Polycarbonate, 40% Glass Reinforced A 40% glass reinforced polycarbonate for maximum mechanical strength and thermal properties. P1443 with UV stabilizer.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 105 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436C40L1 Calcium Reinforced |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® AEN 6000-2 Nylon 6 Engineered Resin |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.40 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1800 43 Natural Nylon 612 with 43% Glass Fiber
(discontinued **) Molded Test Bars: Dry as Molded |
|||
Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm |
2.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF50 FR UV X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightAdditive: Flame Retardant and UV StabilizerFeatures: Flame RetardantAppearance: BlackProcessing Method.. |