Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Nymax™ GMF 600 40 Black 117 V P1 Polyamide 6 (Nylon 6)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer PolyOne Corporation
Trade Name Nymax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ GMF 600 40 Black 117 V P1 Polyamide 6 (Nylon 6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part performance. These materials have been specifically formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Water Absorption 0.80 %

@Thickness 3.18 mm
0.80 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 103 MPa
14900 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 117 MPa
17000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 198 °C

@Thickness 3.18 mm
388 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
Drying Temperature 82.2 °C
180 °F
Descriptive Properties Value Comments
Additive Heat Stabilizer
Appearance Black
Features General Purpose
Heat Stabilized
Filler / Reinforcement GlassMineral, 40% Filler by Weight
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: