PolyOne OnFlex™ V 3040D-S0093 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name OnFlex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne OnFlex™ V 3040D-S0093 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolefin phase with a cross-linked EPDM phase dispersed within it. This range of compounds are specially formulated to provide the melt strength and processability required for blow-moulding processes. In addition to this, OnFlex™-V 3000 series thermoplastic elastomer compounds provide excellent colourability (low yellowness), good mechanical properties, excellent flexibility over a wide temperature range, a wide hardness range, and good hydrocarbon, heat ageing and weather resistance.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ISO 868
Tensile Strength at Break 15.7 MPa
2280 psi
ISO 37
Tensile Stress 7.60 MPa

@Strain 100 %
1100 psi

@Strain 100 %
ISO 37
9.30 MPa

@Strain 300 %
1350 psi

@Strain 300 %
ISO 37
Elongation at Break 570 %
570 %
ISO 37
Compression Set 38 %

@Temperature 23.0 °C,
Time 259000 sec
38 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
60 %

@Temperature 70.0 °C,
Time 79200 sec
60 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
61 %

@Temperature 100 °C,
Time 79200 sec
61 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 3.00 hour
3.00 hour
Descriptive Properties Value Comments
Features General Purpose
Forms Pellets
Generic Material TPE
Generic Material Type Thermoplastic Vulcanizate (TPV)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Fast
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Blow Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: