Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 0.25 %

@Thickness 3.17 mm
0.25 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.4 MPa
6300 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 4.0 - 5.0 %
4.0 - 5.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.30 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
305 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10 - 100 ohm-cm
10 - 100 ohm-cm
ASTM D257
Surface Resistivity per Square 10 - 100 ohm
10 - 100 ohm
ASTM D257
Shielding Effectiveness 30 - 60 dB
30 - 60 dB
1,000 MHz; PolyOne Internal
Processing Properties Metric English Comments
Melt Temperature 238 - 271 °C
460 - 520 °F
Molding