Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 238 - 279 °C | 460 - 535 °F | |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Molding |
PolyOne Lubri-Tech™ PS-30GF/02S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated
(dis Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 238 - 277 °C | 460 - 531 °F | |
PolyOne Stat-Tech™ NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 238 - 268 °C | 460 - 515 °F | |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Melt Temperature | 238 - 268 °C | 460 - 515 °F | |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Melt Temperature | 238 °C | 460 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 238 °C | 460 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 238 °C | 460 °F | Injection |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Melt Temperature | 238 °C | 460 °F | Injection |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Melt Temperature | 238 °C | 460 °F | |
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 238 - 280 °C | 460 - 536 °F | Average value: 257 °C Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |