PolyOne Synprene® RT-3790 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3790 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastomers. These materials are ideal for applications requiring flexibility over a wide temperature range, excellent colorability, broad processing capability and durability.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
ASTM D2240
Tensile Strength at Break 9.38 MPa
1360 psi
510 mm/min; ASTM D412A
Tensile Strength, Yield 5.79 MPa

@Strain 300 %
840 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 560 %
560 %
510 mm/min; ASTM D412A
Resilience 33
33
Bayshore Resilience; ASTM D2632
Tear Strength 36.6 kN/m
209 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Features General Purpose
Forms Pellets
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Consumer Applications
General Purpose
Industrial Applications