Tensile Strength, Yield 5.79 MPa
840 psi
Flatwise (sandwich); Mold Surface
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Strength, Yield 5.79 MPa

@Strain 300 %
840 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Synprene® RT-3790 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength, Yield 5.79 MPa
840 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer
Chemraz® 528 works well in a wide variety of biotechnology and medical device applications where ling-term seal reliability is required. This seal material offers excellent performance in static..