Material Notes:
PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.763 g/cc
1.763 g/cc
ASTM D792
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.4 MPa
5280 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 0.35 %
0.35 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 18.22 GPa
2643 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 68.40 MPa
9921 psi
ASTM D790
Flexural Modulus 19.42 GPa
2816 ksi
ASTM D790
Izod Impact, Notched 0.176 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.329 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity >= 16.0 W/m-K
>= 111 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Surface Resistivity per Square 22000 ohm
22000 ohm
ASTM D257
Descriptive Properties Value Comments
Product Form Pellets