Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Index of Compound 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 35

@Time 15.0 sec
35

@Time 0.00417 hour
Polykemi
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Descriptive Properties Value Comments
Holding Pressure () 20-40
% of injection pressure
Injection Pressure High
Injection Speed () High