Polykemi AB POLYelast TPE RCZ350D UV4 Thermoplastic Elastomer, UV-Resistant

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Polykemi AB
Trade Name POLYelast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE RCZ350D UV4 Thermoplastic Elastomer, UV-Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
With Flow; ISO 2577
0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
Across Flow; ISO 2577
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 97

@Time 15.0 sec
97

@Time 0.00417 hour
Polykemi
Hardness, Shore D 35

@Time 15.0 sec
35

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 14.0 MPa
<= 2030 psi
ISO/R527
Elongation at Break 585 %
585 %
ISO/R527