Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.013 cm/cm @Thickness 3.17 mm |
0.0050 - 0.013 in/in @Thickness 0.125 in |
|
Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66 Non-Hal red phosphorous based Flame Retardant CompoundAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PP HBK15030 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP HBK15030 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH K20020 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS15020 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS4020D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | ASTM D955 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | after bake; ISO 294 |
Solvay Engineered Polymers SEQUEL® 1485 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1485 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, improved scratch and mar .. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH BK901213 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | |
Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Kolon KOPA® KN3311 General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | ASTM D955 |
Kolon KOPEL® KP3755 Specialty TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | |
Lehmann & Voss LUVOCOM® 1-7032-B Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Improved heat resistance.Control disks, cams, sliding elem.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm @Temperature 23.0 °C |
0.0090 - 0.013 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PA6-T25 25% Mineral Filled PA6 Features:Low tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | GB/15585 |
Zhejiang Juner JEPP2056 PP For Automotive Parts Applications: BumpersInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP HBK1501515 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS8020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.011 - 0.013 cm/cm | 0.011 - 0.013 in/in | as molded; ISO 294 |
LyondellBasell INDURE™ X210 TPO Description: INDURE™ X210 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, and processability. Appli.. |