Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Linear Mold Shrinkage 0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
With Flow; ISO 2577
0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Hardness, Shore A 90

@Time 15.0 sec
90

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 12.0 MPa
<= 1740 psi
ISO/R527
Elongation at Break 540 %
540 %
ISO/R527
100% Modulus 0.00950 GPa
1.38 ksi
ISO/R527
300% Modulus 0.0105 GPa
1.52 ksi
ISO/R527
Compression Set 66 %

@Temperature 23.0 °C,
Time 259000 sec
66 %

@Temperature 73.4 °F,
Time 72.0 hour
DIN 53517
80 %

@Temperature 70.0 °C,
Time 86400 sec
80 %

@Temperature 158 °F,
Time 24.0 hour
DIN 53517
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () Low
% of injection pressure
Injection Pressure Low
Injection Speed () High