Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Polykemi AB
Trade Name POLYelast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ISO 1183
Linear Mold Shrinkage 0.017 - 0.024 cm/cm
0.017 - 0.024 in/in
With Flow; ISO 2577
0.017 - 0.024 cm/cm
0.017 - 0.024 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Time 15.0 sec
60

@Time 0.00417 hour
Polykemi
Hardness, Shore D 11

@Time 15.0 sec
11

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 5.00 MPa
<= 725 psi
ISO/R527
Elongation at Break 515 %
515 %
ISO/R527
100% Modulus 0.00100 GPa
0.145 ksi
ISO/R527
300% Modulus 0.00260 GPa
0.377 ksi
ISO/R527
Compression Set 8.0 %

@Temperature 23.0 °C,
Time 259000 sec
8.0 %

@Temperature 73.4 °F,
Time 72.0 hour
DIN 53517
83 %

@Temperature 70.0 °C,
Time 86400 sec
83 %

@Temperature 158 °F,
Time 24.0 hour
DIN 53517
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () Low
% of injection pressure
Injection Pressure Low
Injection Speed () High