Material Notes:
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInformation from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 50

@Time 10.0 sec
50

@Time 0.00278 hour
ASTM D2240
Tensile Stress 1.79 MPa

@Strain 100 %
260 psi

@Strain 100 %
ASTM D412
2.40 MPa

@Strain 300 %
348 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield 3.17 MPa
460 psi
ASTM D412
Elongation at Break 620 %
620 %
ASTM D412
Tear Strength 16.7 kN/m
95.2 pli
ASTM D624