Mechanical Properties Metric English Comments
Tensile Stress 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S EF 70A-3S1975 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Stress 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S EH 70A-3S7004 Thermoplastic Elastomer (TPE)
OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t..
Tensile Stress 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S KA 60A-3S1769 Thermoplastic Elastomer (TPE)
OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Stress 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® F7860 TPE, Fire Retardant
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome..
Tensile Stress 2.40 MPa

@Strain 300 %
348 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2850 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.40 MPa

@Strain 5.00 %,
Temperature 23.0 °C
348 psi

@Strain 5.00 %,
Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..
Tensile Stress 2.40 MPa

@Strain 300 %
348 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P1750 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.40 MPa

@Strain 5.00 %
348 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 5.00 %,
Temperature 23.0 °C
348 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® 4053FG TPC-ET  (Unverified Data**)
Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon..
Tensile Stress 2.40 MPa

@Strain 5.00 %
348 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 103.36 %,
Temperature 120 °C
348 psi

@Strain 103.36 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 5.00 %
348 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 5.00 %
348 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 5.00 %
348 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 124.88 %,
Temperature 200 °C
348 psi

@Strain 124.88 %,
Temperature 392 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 0.360 %,
Time 3.60e+7 sec
348 psi

@Strain 0.360 %,
Time 10000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..
Tensile Stress 2.40 MPa

@Strain 0.201 %,
Time 3600 sec
348 psi

@Strain 0.201 %,
Time 1.00 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..
Tensile Stress 2.40 MPa

@Strain 0.287 %,
Time 360000 sec
348 psi

@Strain 0.287 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..
Tensile Stress 2.40 MPa

@Strain 0.324 %,
Time 3.60e+6 sec
348 psi

@Strain 0.324 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..
Tensile Stress 2.40 MPa

@Strain 0.244 %,
Time 36000 sec
348 psi

@Strain 0.244 %,
Time 10.0 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..
Tensile Stress 2.40 MPa

@Strain 0.444 %,
Time 3.60e+6 sec
348 psi

@Strain 0.444 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 0.558 %,
Time 3.60e+7 sec
348 psi

@Strain 0.558 %,
Time 10000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 0.261 %,
Time 36000 sec
348 psi

@Strain 0.261 %,
Time 10.0 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 0.340 %,
Time 360000 sec
348 psi

@Strain 0.340 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 2.40 MPa

@Strain 0.202 %,
Time 3600 sec
348 psi

@Strain 0.202 %,
Time 1.00 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers