Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 120 MPa
17400 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Tensile Modulus 10.0 GPa
1450 ksi
ISO 527
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 8.20 GPa
1190 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.90 J/cm²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179
2.18 J/cm²

@Temperature -30.0 °C
10.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 168 °C
334 °F
Deflection Temperature at 1.8 MPa (264 psi) 156 °C
313 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Flame Spread 22 mm/min
0.87 in/min
FMVSS302