Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamShine PV3003R2 Acrylonitrile Butadiene Styrene, 10% Carbon Fiber

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PV3003R2 Acrylonitrile Butadiene Styrene, 10% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% Carbon fiber reinforced ABS for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ISO 2577
Melt Flow 22 g/10 min

@Load 10.0 kg,
Temperature 220 °C
22 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
Flexural Strength 110 MPa
16000 psi
ISO 178
Flexural Modulus 6.00 GPa
870 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
IEC 60093
Users viewing this material also viewed the following: