Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamSter RF303G6 PBT, 30% Glass Fiber, Industrial Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industrial Grade, 30% glass fiber reinforced PBT for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Water Absorption at Saturation 0.50 %
0.50 %
ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ISO 2577
Melt Flow 16.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
16.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 130 MPa
18900 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 5.80 GPa
841 ksi
ISO 178
Izod Impact, Notched (ISO) 9.50 kJ/m²
4.52 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Flame Spread 17 mm/min
0.67 in/min
FMVSS302
Glow Wire Test 750 °C
1380 °F
GWFI; IEC 60695
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
864 kV/in
IEC 60250
Users viewing this material also viewed the following: