Material Notes:
Peroxide cured, blue-violet Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage electrical equipment.Applications: For sealing sulphur hexafluoride (SF6) gas in electrical distribution equipment, i.e. medium & high voltage switchgear, also scientific equipment such as X-ray generators, electrostatic particle accelerators and electron microscopes. The specially selected fillers used in this compound provide excellent electrical non-conductive properties to the rubber.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
ASTM D412
Elongation at Break 250 %
250 %
ASTM D412
Compression Set 15 %
15 %
70 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
-45.0 °C
-49.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F