Material Notes:
Peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. To meet ASTM D2000/SAE J200 line call-out M4CA610, A25, B35, C32, EA14, F17. ASTM & ISO designation = EPDM. Tested to 3A requirements.Applications: Excellent water and steam resistance with good compression set properties. Superior heat and chemical resistance compared to sulphur cured EPDM. Not mineral oil resistant.
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
°IRHD; ASTM D1415
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM D412
Elongation at Break 220 %
220 %
ASTM D412
Compression Set 28 %
28 %
22 hours @ 125°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F