Precision Polymer Engineering J70M Butyl Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering J70M Butyl Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bromobutyl Rubber, 65-75 IRHD. Brominated isobutylene-isoprene copolymer. To meet BS3227 Grade 70 and ASTM D2000 line call-out MBA708, F17.Applications: Bromobutyl is resistant to the same fluids as Ethylene Propylene (EPDM). It has excellent resistance to gas permeation. Except for its gas permeation resistance, Butyl is considered to be inferior to EPDM for O-Ring service.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
55 - 85
55 - 85
°IRHD, ±15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM D412
6.30 - 11.7 MPa
914 - 1700 psi
±30% change after 70 hours @ 100°C; ASTM D412
Elongation at Break 175 %
175 %
-50% change after 70 hours @ 100°C; ASTM D412
350 %
350 %
ASTM D412
Compression Set 40 %
40 %
72 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F