Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering F70A Fluorosilicone Rubber Blue Fluorosilicone Rubber, 60 to 70 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, .. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N70Z Nitrile Rubber Carboxylated Nitrile Butadiene Rubber (XNBR), 65-75 °IRHD. Terpolymer of acrylonitrile, butadiene and methacrylic acid.Applications: Carboxylated Nitrile (XNBR) offers much higher modulus, increas.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N80M Nitrile Rubber Nitrile Rubber, 75-85 °IRHD. Meets British Standard BS2751 BA80. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR.Applicat.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N90L Nitrile Rubber Low Nitrile Rubber, 85-95 °IRHD. Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. ASTM D2000 line call-out M6BG907, A14, B.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering R50Y Natural Rubber Non-black, Natural Rubber, 45-55 °IRHD. Formulated to meet BS1154 Grade Y50. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber and is reinforced using zinc.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering R70Z Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to meet BS1154 Grade Z70. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S50E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S55T Silicone Rubber Translucent Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United Sta.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60Z Silicone Rubber Grey Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Fo.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65B Silicone Rubber Low Compression Set, Black Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compr.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65Y Silicone Rubber Golden Yellow, Silicone 55-65 °IRHD. Diesel liner ring grade. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and low temperature flexibility combined with low compression set.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S70B Silicone Rubber Black Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and .. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S71U Silicone Rubber Translucent Silicone Rubber, 70-75 °IRHD. Platinum cured Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Silicone compound in conformity with the requirement.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S75T Silicone Rubber Translucent Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. Silicone compound in conformity with.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S80U Silicone Rubber Translucent Silicone Rubber, 70 -80 °IRHD. Shore A Platinum cured Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Silicone compound in conformity with the req.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z70B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Butadiene Rubber (HNBR), 65-75 °IRHD. Medium acrylonitrile content (ACN = 34%). To meet ASTM D2000/SAE J200 line call-out M4DH716, A26, B36, EO16, EO36, F17.A.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z70F Hydrogenated NBR Compound Hydrogenated Nitrile Butadiene Rubber (HNBR), 65-75 °IRHD. Medium acrylonitrile content (ACN = 34%). Formulated using only those ingredients determined by the United States Food and Drug Administr.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z75R Hydrogenated NBR Compound Red Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5.Ap.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z85L Hydrogenated NBR Compound Peroxide Cured, Hydrogenated Nitrile Rubber, 81-90 °IRHD. Low acrylonitrile content.Applications: Specially compounded for service in low-temperature applications. High strength and excellent chem.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z85T Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 80-90 °IRHD. Medium acrylonitrile content (ACN =36%). ASTM D2000 line call-out M2DH920, A26, B16, EO16, EO36, F14, Z1, where Z1 = Hardness 80-90.Appli.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z95X Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applica.. |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |