Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering R90B Natural Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering R90B Natural Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural Rubber, 85-95 °IRHD. This material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applications: Natural rubber offers low compression set, high tensile strength, high resilience and excellent resistance to tear and abrasion.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
°IRHD; ASTM D1415
75 - 105
75 - 105
°IRHD, ±15 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
ASTM D412
5.60 - 10.4 MPa
812 - 1510 psi
±30% change after 168 hours @ 70°C; ASTM D412
Elongation at Break 100 %
100 %
-50% change after 168 hours @ 70°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 50 %
50 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Flash Point >= 300 °C
>= 572 °F
Users viewing this material also viewed the following: