Precision Polymer Engineering S60X Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering S60X Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Red Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Specially compounded to provide the optimum retention of physical properties whilst operating in extreme high temperature applications.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
75
75
°IRHD, +15 change after 48 hours @ 315°C; ASTM D1415
Tensile Strength, Yield 3.75 MPa
544 psi
-50% change after 48 hours @ 315°C; ASTM D412
7.50 MPa
1090 psi
ASTM D412
Elongation at Break 87.5 %
87.5 %
-75% change after 48 hours @ 315°C; ASTM D412
350 %
350 %
ASTM D412
Compression Set 20 %
20 %
24 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-60.0 °C
-76.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F