Precision Polymer Engineering S60Y Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering S60Y Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Yellow Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600. ASTM & ISI designation = VMQ.Applications: Excellent heat resistance and low temperature flexibility. Used primarily for dry heat static seals. Low physical strength and poor abrasion resistance prevents dynamic sealing.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
50 - 70
50 - 70
°IRHD, ±10 change after 70 hours @ 225°C; ASTM D1415
Tensile Strength, Yield 6.00 MPa
870 psi
-25% change after 70 hours @ 225°C; ASTM D412
8.00 MPa
1160 psi
ASTM D412
Elongation at Break 220 %
220 %
-45% change after 70 hours @ 225°C; ASTM D412
400 %
400 %
ASTM D412
Compression Set 30 %
30 %
24 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-60.0 °C
-76.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F