Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PREFLEX E100 Polyphenylene Ether (PPO/PPE)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer Premix Thermoplastics Inc.
Trade Name PREFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PREFLEX E100 Polyphenylene Ether (PPO/PPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material are available and marketed under the name PREBOARD. Thus the same material can also be used in rigid/flex boards. The material lends itself also well for injection moulding and is available for that purpose in granules sold under the name PREPERM. This enables the production of 3D circuit boards. Key features: Low dissipation factorLow dielectric constant Low water absorptionHigh TgZero shrinkage even at 190°CLow CTE in all directionsExcellent adhesion with inks and adhesivesExcellent chemical resistanceMinimum thicknesses below 10 micronsRecyclable and RoHS compliantNon halogen flame retardant grades also availableApplications: Flexible printed circuits, printed electronics, fuel cells and other uses calling for a special film.Information from Premix OY
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Thickness 100 microns
3.94 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 48 %
48 %
Film Elongation at Break, TD 32 %
32 %
Film Tensile Strength at Break, MD 52.0 MPa
7540 psi
Film Tensile Strength at Break, TD 46.0 MPa
6670 psi
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 210 °C
410 °F
Shrinkage, MD 1.0 %
1.0 %
0.00 %

@Temperature 190 °C,
Time 7200 sec
0.00 %

@Temperature 374 °F,
Time 2.00 hour
Shrinkage, TD 0.10 %
0.10 %
0.00 %

@Temperature 200 °C,
Time 600 sec
0.00 %

@Temperature 392 °F,
Time 0.167 hour
Electrical Properties Metric English Comments
Dielectric Constant 2.55

@Frequency 1.00e+9 - 1.00e+10 Hz
2.55

@Frequency 1.00e+9 - 1.00e+10 Hz
Dissipation Factor 0.00050

@Frequency 1.00e+9 - 1.00e+10 Hz
0.00050

@Frequency 1.00e+9 - 1.00e+10 Hz
Processing Properties Metric English Comments
Moisture Content <= 0.20 %