Physical Properties Metric English Comments
Thickness 100 microns
3.94 mil
Premix Thermoplastics PREFLEX E100 Polyphenylene Ether (PPO/PPE)
PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material ..
Thickness >= 100 microns
>= 3.94 mil
Bondline thickness
Parker Chomerics THERM-A-GAP™ GEL 30 High Performance Fully Cured Dispensable Gel
Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl..
Thickness 100 microns
3.94 mil
Standard
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Thickness 100 - 127 microns
3.94 - 5.00 mil
Available Range
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Thickness >= 100 microns
>= 3.94 mil
Minimum Web
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Thickness 100 microns
3.94 mil
As Tested
Solvay Specialty Polymers Ajediumâ„¢ Film Thermoplastic Polyimide (PI, TP)
TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior ra..
Thickness 100 microns
3.94 mil
Shandong Dongyue Shenzhou New Material Co CHFM 100 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Thickness 100 microns
3.94 mil
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC)
TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo..
Thickness <= 100 microns
<= 3.94 mil
Per single coat
Daikin NEOFLON AC-5600 PFA Coating Powder, White
NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Up to a thickness of 100 microns per single coat.Proces..
Thickness <= 100 microns
<= 3.94 mil
Per single coat
Daikin NEOFLON NC-1500 FEP Coating Powder, White
NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Up to a thickness of 100 microns per single coat.Proc..
Thickness 100 microns
3.94 mil
Typical Wall Thickness
COI Ceramics Al2O3SiO2 Oxide Hollow Spheres
Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres tha..
Thickness 100 microns
3.94 mil
Typical Wall Thickness
COI Ceramics SiC Hollow Spheres
Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres tha..
Thickness 100 microns
3.94 mil
Carmel Olefins IPETHENE® 100 Low Density Polyethylene
IPETHENE® 100 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, good processability and good ESCR. APPLICATIONS IPETHENE® 100 is used for production..
Thickness 100 microns
3.94 mil
Carmel Olefins IPETHENE® 4203 Low Density Polyethylene
IPETHENE® 4203 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, very good bubble stability in thick-gauge blown film processing, and excellent ESCR. ..
Thickness 100 - 140 microns
3.94 - 5.51 mil
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric
P & P Technology material reference NF32B050A21 is a metalised conductive fabric designed for use in EMC shielding and in the manufacture of conductive EMC gaskets. The material is a rip-stop weave ..