Protective Coating PC-Woody® Epoxy Paste

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Protective Coating Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Protective Coating PC-Woody® Epoxy Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC-WOODY® is an epoxy paste formulated to replace missing and rotted wood with structural strength greater than most wood. Use for permanent repairs on all types of wood-exterior or interior. Unlike typical wood fillers, PC-WOODY® is a permanent wood repair product.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.720 g/cc
0.0260 lb/in³
ASTM D792
Water Absorption 0.44 %
0.44 %
ASTM C413
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
1 Week Cure; ASTM D2240
Elongation at Break 5.0 - 7.0 %
5.0 - 7.0 %
ASTM D638
Flexural Yield Strength 9.00 MPa
1310 psi
ASTM D580
Compressive Yield Strength 16.0 MPa
2320 psi
ASTM D695
Adhesive Bond Strength 5.90 MPa
856 psi
Tensile Shear Strength; ASTM D1002
Gardner Impact 11.0 J
8.11 ft-lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648