Polymer Property : Flexural Yield Strength = 1310 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 9.00 MPa
1310 psi
ASTM D580
Protective Coating PC-Woody® Epoxy Paste
PC-WOODY® is an epoxy paste formulated to replace missing and rotted wood with structural strength greater than most wood. Use for permanent repairs on all types of wood-exterior or interior. Unl..
Flexural Yield Strength 9.00 - 352 MPa

@Temperature -40.0 - 200 °C
1310 - 51100 psi

@Temperature -40.0 - 392 °F
Average value: 119 MPa Grade Count:22
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Yield Strength 9.00 - 90.0 MPa

@Temperature 125 - 275 °C
1310 - 13100 psi

@Temperature 257 - 527 °F
Average value: 42.2 MPa Grade Count:8
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..