Pyrotek MCX-40 Insulating Board

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek MCX-40 Insulating Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MCX-40 is a bonded-mica composite for use in glass contact applications. Its high operating temperature, low porosity, and low thermal conductivity make it ideal for all areas of hot glass transfer, including takeout jaws/inserts, sweep out pads, lehr loader bar pads/inserts, and high temperature flat glass quench rollers.ApplicationsGlass contact insulating material AdvantagesAbrasion resistant Non-marking to glass Low porosity Resists oxidizing atmospheres better than carbon or graphite Machinable with standard equipment High-impact strength Can be molded to net shape based on consumer specifications Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.491 g/cc
0.08999 lb/in³
Water Absorption 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength 90.0 MPa
13100 psi
Compressive Strength 310 MPa
45000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.420 W/m-K
2.91 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 510 °C
950 °F
Continuous