Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Pyroboard™ S1300 Roller

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Pyroboard™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyroboard™ S1300 Roller.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyroboard™ S1300 was developed specifically for use in hotter zones of an annealing furnace.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.833 g/cc
0.0301 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.86 MPa
270 psi
Flexural Strength 3.45 MPa
500 psi
Compressive Strength 3.10 MPa
450 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.0677 W/m-K
0.470 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1260 °C
2300 °F
Shrinkage 3.50 %

@Temperature 982 °C
3.50 %

@Temperature 1800 °F
Thickness
4.80 %

@Temperature 982 °C
4.80 %

@Temperature 1800 °F
Surface
10.2 %

@Temperature 1204 °C
10.2 %

@Temperature 2199 °F
Surface
10.6 %

@Temperature 1204 °C
10.6 %

@Temperature 2199 °F
Thickness
Users viewing this material also viewed the following: