Material Notes:
Pyrocast SCM-2600 is suited for use in aluminum applications where severe wear is a factor. It is a high purity silicon carbide based refractory with low cement content.ApplicationsHigh erosion areas of aluminum transfer launders Aluminum tapout blocks in melting and holding furnaces Baffles AdvantagesHigh wear resistance High thermal conductivity Resistant to molten metal Low iron content Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.563 g/cc
0.09259 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0170 GPa

@Temperature >=110 °C
2.47 ksi

@Temperature >=230 °F
0.0240 GPa

@Temperature 816 °C
3.48 ksi

@Temperature 1500 °F
Thermal Properties Metric English Comments
Thermal Conductivity 6.60 W/m-K

@Temperature 538 °C
45.8 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6.66 W/m-K

@Temperature 260 °C
46.2 BTU-in/hr-ft²-°F

@Temperature 500 °F
7.19 W/m-K

@Temperature 816 °C
49.9 BTU-in/hr-ft²-°F

@Temperature 1500 °F
7.80 W/m-K

@Temperature 1093 °C
54.1 BTU-in/hr-ft²-°F

@Temperature 1999 °F
Maximum Service Temperature, Air 1427 °C
2601 °F
Shrinkage 0.100 %

@Temperature 816 °C
0.100 %

@Temperature 1500 °F
Linear
Component Elements Properties Metric English Comments
Al2O3 7.9 %
7.9 %
CaO 2.2 %
2.2 %
Other 6.9 %
6.9 %
SiC 76.7 %
76.7 %
SiO2 6.3 %
6.3 %