Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1427 °C
2601 °F
Continuous
Pyrotek L4 Fiber Seal Pre-cut Gasket
A lightweight needled blanket which is strong and durable.Information provided by Pyrotek.
Maximum Service Temperature, Air 1427 °C
2601 °F
Pyrotek L-4 Fiberseal Blanket
Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation p..
Maximum Service Temperature, Air 1427 °C
2601 °F
Continuous
Pyrotek L6 Fiber Seal Pre-cut Gasket
A lightweight needled blanket which is strong and durable.Information provided by Pyrotek.
Maximum Service Temperature, Air 1427 °C
2601 °F
Pyrotek L-8 Fiberseal Blanket
Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation p..
Maximum Service Temperature, Air 1427 °C
2601 °F
Pyrotek L-6 Fiberseal Blanket
Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation p..
Maximum Service Temperature, Air 1427 °C
2601 °F
Continuous
Pyrotek L8 Fiber Seal Pre-cut Gasket
A lightweight needled blanket which is strong and durable.Information provided by Pyrotek.
Maximum Service Temperature, Air 1427 °C
2601 °F
Continuous
Pyrotek M-6 Fiber Seal Pre-cut Gasket
Contains no binders and is not changed by exposure to high temperatures.Information provided by Pyrotek.
Maximum Service Temperature, Air 1427 °C
2601 °F
Pyrotek M-6 Fiberseal Blanket
Stitched with high-temperature fibers. Contains no binders. Not changed by exposure to high temperatures.Dimensions610 mm x 7.6 m25 mm thickApplicationsHigh-temperature gaskets Furnace linings Gen..
Maximum Service Temperature, Air 1427 °C
2601 °F
Continuous
Pyrotek M-8 Fiber Seal Pre-cut Gasket
Contains no binders and is not changed by exposure to high temperatures.Information provided by Pyrotek.
Maximum Service Temperature, Air 1427 °C
2601 °F
Pyrotek Pyrocast SCM-2600 High Wear Impact Refractory Castable
Pyrocast SCM-2600 is suited for use in aluminum applications where severe wear is a factor. It is a high purity silicon carbide based refractory with low cement content.ApplicationsHigh erosion are..
Maximum Service Temperature, Air 1427 °C
2601 °F
Zircar Ceramics AXHTM Alumina-Silica Insulation
ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a..
Maximum Service Temperature, Air 1427 °C
2601 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Fibermax® Caulk
Fibermax caulk is a high-temperature blend of Fiberfrax bulk fibers, Fibermax polycrystalline high-alumina fibers, and inorganic binder. This product is available in convenient-to-use caulking tube..
Maximum Service Temperature, Air 1427 °C
2601 °F
Zircar Ceramics ASB-2600 Alumina-Silica Blanket
Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics.
Maximum Service Temperature, Air 1427 °C
2601 °F
BNZ Materials Blazecrete 2600 Dense Castable
Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as..
Maximum Service Temperature, Air 1427 °C
2601 °F
Normal oxidizing atmosphere
BNZ Materials BNZ-26 HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Maximum Service Temperature, Air 1427 °C
2601 °F
Normal oxidizing atmosphere
BNZ Materials BNZ-26 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Maximum Service Temperature, Air 1427 °C
2601 °F
Normal oxidizing atmosphere
BNZ Materials BNZ-26-60 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Maximum Service Temperature, Air 1427 °C
2601 °F
BNZ Materials PA 26 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Maximum Service Temperature, Air 1427 °C
2601 °F
BNZ Materials Bazelite 2600 LI Insulating Castable
Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov..
Maximum Service Temperature, Air 1427 °C
2601 °F
Pyrotek M-4 Fiberseal Blanket
A white high-temperature felt.Dimensions610 mm x 15.2 m25 mm thickApplicationsGaskets Trough covers Trough gaskets Information provided by Pyrotek.
Maximum Service Temperature, Air 1427 °C
2601 °F
Pyrotek M-8 Fiberseal Blanket