Pyrotek RFM Light density refractory composite material

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek RFM Light density refractory composite material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The RFM material is a composite made of fiberglass fabric and a wollastonite slurry. It can be shaped to very complex and thin parts. It has a very good behavior against molten aluminum alloys.ApplicationsDistribution troughs for continuous casting machine Rigid molten metal distributor Float bottom part Casting tip Auto pour ladle AdvantagesNo pre-heating required Excellent mechanical properties Excellent resistance to erosion Can be molded Non-wetting by molten aluminum High temperature service Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0214 GPa
3.10 ksi
Thermal Properties Metric English Comments
CTE, linear 0.900 µm/m-°C

@Temperature 20.0 °C
0.500 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.430 W/m-K

@Temperature 500 °C
2.98 BTU-in/hr-ft²-°F

@Temperature 932 °F
Maximum Service Temperature, Air 1100 °C
2010 °F