Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Quadrant Engineering Plastics Products
Trade Name Quadrant
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Water Absorption <= 0.040 %
<= 0.040 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.040 %
<= 0.040 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
ASTM D2240
Tensile Strength 57.6 MPa
8350 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Tensile Modulus 3.21 GPa
465 ksi
ASTM D638
Flexural Strength 57.6 MPa
8350 psi
ASTM D790
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
Compressive Strength 82.7 MPa
12000 psi
10% Def.; ASTM D695
Compressive Modulus 2.41 GPa
350 ksi
ASTM D695
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256 Type A
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C
116 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+12 ohm
>= 1.00e+12 ohm
ASTM D257
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Limited
Limited
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Limited
Limited
Hydrocarbons - Aromatic Limited
Limited
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Descriptive Properties Value Comments
Machinability 6
1-10, 1=Easier to Machine