Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | |
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | ASTM D257 |
Ovation Polymers Nemcon™ H PC DP113/X5 Polycarbonate Polycarbonate-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | per cm square at 50% humidity; ASTM D257 |
Network Polymers PC-1029 AS/P Description: Antistatic PolycarbonateInformation provided by Network Polymers Inc. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257-91 |
NeXolve LaRC™-CP1 Polyimide Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptak.. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257 |
Quadrant EPP Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257 |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-10CP/000 Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:AntistaticConductive Carbon Powder FilledInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | VDE 0303 |
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Conditioned |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+12 ohm | 1e+05 - 1.00e+12 ohm | ASTM D257 |
Kostat KAH1 Heat Seal Activated Cover tapes KOSTATs KAH1 series of Heat Seal Activated Cover Tape is manufactured using Antistatic Polyethylene Terephthalate film and other proprietary adhesive materials. The component for its anti-static pr.. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | VDE 0303 |
GEHR Plastics PA 6.6 Nylon 6.6, Conditioned |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | ASTM D257 |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257 |
Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+12 ohm | 1e+05 - 1.00e+12 ohm | ASTM D257 |
PolyOne Edgetek® AM-10CF-20GF/000 HS Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |