Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quantum Composites QC-7810 55% Glass Fiber Polyester SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites QC-7810 55% Glass Fiber Polyester SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QC-7810 is a toughened thermoset polyester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and flame resistance. It is suggested for applications subject to impacts and rough handling. QC-7810 has Underwriter's Laboratory recognition for 130°C use. Form and Color = Rolled Sheet, Black. Glass Fiber Length = .5 inchData provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 68
68
ASTM D2583
Tensile Strength, Ultimate 324 MPa
47000 psi
ASTM D638
Flexural Yield Strength 482 MPa
69900 psi
ASTM D790
Flexural Modulus 17.2 GPa
2490 ksi
ASTM D790
Izod Impact, Notched 17.0 J/cm
31.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
UL Recognized
>= 260 °C
>= 500 °F
Deflection Temp; Load not reported; ASTM D648
Flammability, UL94 V-1

@Thickness 2.90 mm
V-1

@Thickness 0.114 in
Shrinkage 0.0010 %
0.0010 %
Processing Properties Metric English Comments
Processing Temperature 132 - 149 °C
270 - 300 °F
Mold temperature