Izod Impact, Notched 17.0 J/cm
31.8 ft-lb/in
ASTM D256
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC  (discontinued **)
QC-7810 is a toughened thermoset polyester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and flame resistance. It is suggested..