R70-068 Styrene-based Biomedical Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF R70-068 Styrene-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
ASTM D2240
Tensile Strength, Ultimate 11.2 MPa
1630 psi
ASTM D412
Tensile Strength, Yield 0.965 MPa
140 psi
at 100%; ASTM D412
Elongation at Break 850 %
850 %
ASTM D412
Tear Strength 19.3 kN/m
110 pli
die B; ASTM D624
Compression Set 38 %
38 %
ASTM D395