Tensile Strength, Yield 0.965 MPa
140 psi
at 200%, post cured- 2 hours at 177°C
Multibase SILASTIC® C7-4535 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 0.965 MPa
140 psi
ISO 527-2
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Tensile Strength, Yield 0.965 MPa
140 psi
at 200%, molded-without post cure; ASTM D412
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 0.965 MPa
140 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 5862 Fluoro-silicone
Fluoro-siliconeInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 0.965 MPa
140 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3805M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer..
Tensile Strength, Yield 0.965 MPa
140 psi
at 100%; ASTM D412
R70-068 Styrene-based Biomedical Elastomer
Tensile Strength, Yield 0.965 MPa
140 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® ST-6105 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs..