Radici Radilon® N66-SRV130 Nylon 66  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® N66-SRV130 Nylon 66  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.95 %
0.95 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 115 MPa
16700 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Modulus of Elasticity 5.45 GPa
790 ksi
ASTM D638
Flexural Yield Strength 150.0 MPa
21750 psi
ASTM D570
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
ASTM D648
Flammability, UL94 HB
HB
UL94