Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Enviramid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Water Absorption 1.2 %
1.2 %
Saturation, Immersed; ASTM D570
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 71.7 MPa
10400 psi
ASTM D790
Flexural Modulus 2.300 GPa
333.6 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved