Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Reliance Industries PBT - 35% Glass filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries PBT - 35% Glass filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Reliance Industries
Physical Properties Metric English Comments
Specific Gravity 1.59 g/cc
1.59 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103 MPa
14900 psi
Tensile Modulus 8.27 GPa
1200 ksi
Flexural Strength 193 MPa
28000 psi
Flexural Modulus 8.27 GPa
1200 ksi
Izod Impact, Notched 6.99 J/cm
13.1 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 °C
424 °F