Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV MX 2230 is a one-component acrylate based polymer designed to be used as a quick-fixture, surface activated adhesive, (with optional UV or oven cure), for applications on a variety of substrates where two surfaces can be mated together. This easy to use formulation can be fixtured in seconds after exposure to UV MX 2230 Surface Activator. After gel, (usually in less than one to two minutes), the product can withstand mild handling and defixturing. A secondary heat cure or UV cure is optional to complete the polymerization process, yielding a product with good dimensional stability, excellent chemical resistance and outstanding bond strength.Applications: Ideal for those applications that require the on-line fixture speed of an activated acrylic and the versatility of a conventional; one-part cure.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Viscosity 1500 cP

@Temperature 25.0 °C
1500 cP

@Temperature 77.0 °F
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Cured
Elongation at Break 20 %
20 %
Cured
Shear Strength 8.69 MPa
1260 psi
Cured, tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Cured
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Cured
Electrical Properties Metric English Comments
Dielectric Strength 16.5 kV/mm
420 kV/in
Cured
Descriptive Properties Value Comments
Color Clear to amber
Peel Shear Strength 30 in/lbs